TM-25659 |CAS 260553-97-7

Two-step K⁺/Rb⁺ ion exchange enabling high mechanical properties and brittle-ductile transition in 3D-printed dental lithium disilicate

Zengqi Ye, Xin Zhou, Qianshu Xia, Xuanbing Chen, Xiaofeng Lu, Qian Teng, Tianxiang Ren, Xian Tong, Zhaoping Chen, Yuncang Li, Li Zhu, Cuie Wen, Jixing Lin, Jianfeng Ma

Journal:JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY

IF:16.8

DOI:10.1016/j.jmst.2026.05.052

PMID:

Published:2026-06-03

research field:牙科材料增材制造材料科学机械工程

Abstract

To improve the mechanical reliability of thin-walled lithium disilicate (LD) veneers, this study developed a strengthening strategy that integrates vat photopolymerization (VP) with a two-step ion-exchange (IE) process. VP was employed to fabricate thin-walled LD structures, eliminating machining-induced damage, while a sequential K⁺/Rb⁺ IE process achieved both sufficient IE depth and compressive stress, overcoming their conventional trade-off. The two-step IE process increased the flexural strength of LD by 52.0% to 448.6 ± 31.5 MPa and improved the fracture toughness by 80.4% to 2.64 ± 0.10 MPa m 1/2 . The significant enhancement in mechanical performance was mainly attributed to a 349% increase in compressive stress (CS), reaching 141.9 ± 4.4 MPa. The atomic force microscope revealed that the ultrahigh CS was attributed to the volumetric expansion of an amorphous phase. Under scratching loads of 100 mN above the brittle-ductile transition threshold (∼70 mN), the coefficient of friction of IE-processed LD increased by nearly 50%, indicating a transition in energy dissipation from brittle crack initiation to localized plastic deformation. Overall, the VP-fabricated LD, after undergoing the two-step IE processing, exhibits markedly enhanced strength and toughness. This improved mechanical performance effectively resists crack initiation and propagation caused by sharp contacts, thereby contributing to the superior long-term reliability of the LD veneers in the oral masticatory environment.